NORMETPan India Project Distributor

Normet TamPur 150 (ECO Range) — Hydrophilic Flexible PU Grout for Moving Cracks and Joints

A single-part hydrophilic polyurethane that reacts with water to form a tight, elastic seal with over 120% elongation. Used for cracks, fractures and joints that keep moving, and as the flexible second pass after a rigid water stop.

BrandNormetCategoryInjection resins & micro cementsFormSingle-component hydrophilic PU prepolymer (inject neat or 1:1 with water)

What is it?

A one-part hydrophilic polyurethane prepolymer from Normet’s ECO range. On contact with water it forms a flexible, impermeable elastomeric seal.

Where is it used?

Leaking cracks, fractures and joints in concrete, brick and mortar, especially those that move.

Why use it?

Elongation above 120% and tensile strength above 1.65 MPa (ASTM D638), excellent adhesion, and resistance to most solvents, mild acids and alkalis.

How is it applied?

Inject neat with a single-component high-pressure pump, or with a twin-piston pump mixing water and resin to vary foam density.

About Normet TamPur 150 (ECO Range)

Normet TamPur 150 (ECO Range) is the flexible grade of the TamPur family. Unlike the hydrophobic grades, it is hydrophilic: it takes water into its structure as it reacts, forming a resilient elastomeric seal rather than a rigid foam. It can be injected directly into a leaking crack, fracture or joint, or mixed 1:1 with water during injection.

Because the cured seal stretches and recovers, TamPur 150 is suited to joints and cracks that open and close with temperature or load. Normet also names it as a second-pass option after TamPur 100 where a flexible seal is needed. Space Arc Engineering supplies it as the Pan India Project Distributor of NORMET, with trial and site support.

The technical insight

Hydrophilic and hydrophobic grouts solve different problems. A hydrophobic foam (like TamPur 100) pushes water out and sets hard; a hydrophilic prepolymer like TamPur 150 binds water into a soft, elastic polymer. That gives lower expansion (a free-rise ratio of 2 to 3.5 times) but much better flexibility: elongation above 120% and tensile strength above 1.65 MPa in thin sections (ASTM D638). Reaction starts very quickly, with a cream time of about 4 seconds, and rise times of 80–240 seconds depending on temperature and water ratio. Using a twin-piston pump, the water-to-resin ratio can be changed from 1:1 to 1:4 to adjust foam density. The grout also holds up against most organic solvents, mild acids and alkalis, and reacts with seawater.

Where it is used

  • Sealing leaking cracks that move with temperature or load
  • Flexible sealing of construction and expansion-affected joints
  • Leaking fractures in concrete, brick and mortar
  • Second-pass flexible seal after a rigid water-stop grout
  • Marine and coastal structures with seawater
  • Pipe and service penetrations with some movement
  • Basement walls and tunnel joints with recurring leaks

Key advantages

  • Flexible elastomeric seal: elongation above 120% (ASTM D638)
  • Tensile strength above 1.65 MPa (ASTM D638)
  • Excellent adhesion to concrete, brick and mortar
  • Resistant to most organic solvents, mild acids and alkalis
  • Very fast start: cream time about 4 seconds
  • Reacts even with seawater or mineral water
  • Can be injected neat or mixed with water at varying ratios
  • Environmentally friendly (ECO range)

Limitations & considerations

  • Low free-rise ratio (2–3.5 times), so it is not meant to fill voids; Normet points to TamPur 117 for that
  • Strong, fast-flowing leaks may need a rigid first pass (such as TamPur 100) before the flexible seal
  • Crystallisation can occur below 10°C; indirect heating and mixing restores the liquid
  • Condition for 12 hours before use and mix for 15 seconds to make it uniform
  • Rise time lengthens in cold conditions (240 seconds at 10°C)
  • Laboratory data; site behaviour depends on water, temperature and crack width

Selection & best practice

Assess the leak and crack movement first. For moderate leaks, inject TamPur 150 neat with a single-component high-pressure pump; it reacts with water in the structure. Where you need to control foam density, use a twin-piston pump and set the water-to-resin ratio (from 1:1 to 1:4 in Normet’s table). For heavy running water, cut the flow with a rigid grout first and follow with TamPur 150 as the elastic seal.

Condition the material for at least 12 hours and mix with a clean, dry drill and paddle for at least 15 seconds before use. In cold weather, warm the pail indirectly if crystals form and remix. Store between 10°C and 38°C, dry and out of direct sun.

Specifications

ChemistrySingle-component hydrophilic polyurethane prepolymer (polyether polyols); flexible elastomeric seal
AppearanceYellow liquid
Viscosity at 25°C150–400 mPa·s (Brookfield DV II, spindle 2, 60 rpm)
Density at 25°C1.1
Elongation, thin section (ASTM D638)> 120%
Tensile strength (ASTM D638)> 1.65 MPa
Reaction at 25°C, water:resin 1:1Cream 4 s; rise 120 s; free rise ratio 2–2.5×
Water:resin ratios (25°C)1:1 to 1:4; rise 80–130 s; free rise 2× to 3.5×
Rise time vs temperature (1:1)240 s at 10°C; 150 s at 20°C; 80 s at 30°C
Packaging20 kg metal pail
Storage / shelf life10–38°C, dry, out of direct sunlight; one year unopened

Values as per Normet’s published TDS (Australia edition, V4AU dated 20 Feb 2025). Figures are typical laboratory results; we recommend a site trial to confirm suitability.

Industry use cases

Metro & Rail Tunnels

Flexible sealing of segment joints and cracks that move with traffic vibration and temperature.

Basements & Podiums

Permanent elastic seal on recurring leaks at joints and shrinkage cracks.

Coastal & Marine Works

Leak sealing where the water is saline.

Water Structures

Second-pass flexible sealing after rigid water-stop injection in tanks and channels.

Frequently asked questions

What is the difference between hydrophilic and hydrophobic PU grout?
Hydrophobic grouts such as TamPur 100 foam strongly and set rigid. Hydrophilic TamPur 150 takes water into its structure and forms a flexible, elastic seal that can move with the crack.
Can TamPur 150 be used after TamPur 100?
Yes. Normet suggests a second pass with a flexible grout such as TamPur 150 after TamPur 100 where a flexible seal is needed.
How flexible is the cured seal?
Normet’s TDS gives elongation above 120% and tensile strength above 1.65 MPa (ASTM D638, thin section).
Does it need to be mixed with water before injection?
Not necessarily. It can be injected neat and react with water in the crack, or injected with water using a twin-piston pump at ratios from 1:1 to 1:4.
What happens if it crystallises in cold weather?
Below 10°C crystallisation may occur. Normet states that indirect heating and mixing returns the liquid to its original form.

How we position Normet TamPur 150 (ECO Range)

Choose TamPur 150 (ECO Range) when the crack or joint will keep moving and you need an elastic, long-term seal, or as the flexible second pass after a rigid water stop. If water is running hard, stop it first with TamPur 100 (catalyst-adjusted, high expansion) or TamPur 125 (ECO Range) (two-part ECO). For semi-flexible foam with more expansion, consider TamPur 130 (ECO Range) or TamPur 136. When strength or slab stabilisation is the aim, use TamPur 120. For rock and soil consolidation, use TamPur 116T; for curtain grouting with acrylic resins, see TamAcryl 3000 and TamAcryl 2000. Browse the full Normet range or our waterproofing solutions.

Not sure which grade fits? Send us photos of the leak or ground condition, the flow rate and the site temperature. Our team will suggest a grade and help plan a trial.

Source Normet TamPur 150 (ECO Range) for your project

Pan India Project Distributor of NORMET. Technical support for trials, dosage optimisation and site support across Delhi NCR and Pan India.

Scroll to Top