Normet TamCrete HF — High Flow, High Strength Non-Shrink Cementitious Grout
A free-flowing, chloride-free precision grout for gaps of 5 mm to 75 mm under bridge bearings, crane rails, turbines and precast beams — 70 MPa at 28 days as per Normet’s TDS, supplied Pan India by Space Arc.
What is it?
A pre-bagged, non-shrink cementitious grout made with non-reactive aggregate (maximum 2 mm) and low-alkali, shrinkage-compensated Portland cement. Only clean water is added on site.
Where is it used?
Bridge bearing plinths, crane rail bedding, holding-down bolts and starter bars, bedding of precast beams, machinery and turbine bases, and repairs to spalled or cracked concrete.
Why use it?
High flow lets it fill long, narrow gaps from one side, while controlled expansion, 70 MPa ultimate strength and resistance to vibration, impact, oil and water suit heavy dynamic loads.
How is it applied?
Pour or pump into a saturated surface-dry, formed gap from one side only, in one uninterrupted pour, then cure straight away with a curing compound or taped polythene.
About Normet TamCrete HF
Normet TamCrete HF (“Tamcrete HF” in many searches) is a high-flow, high-strength cementitious grout for precision bedding. Where a general purpose grout suits open base plates, HF is designed for the harder jobs: long flow paths, tight clearances, pumped placement and equipment that vibrates or takes impact. Its maximum aggregate size of 2 mm and controlled expansion let it fill gaps of 5–75 mm without shrinking away from the steel.
Because it is pre-bagged and needs only water, quality on site depends mostly on water control, surface preparation and continuous placement. Space Arc Engineering, Pan India Project Distributor of NORMET, supplies TamCrete HF and offers technical support for trial pours and site set-up, so the first bearing or base plate is right.
The technical insight
Flowability and strength usually pull in opposite directions: more water flows better but weakens the grout and causes bleed and settlement. TamCrete HF gets around this with a dispersing admixture system and graded fine aggregate, giving a free water/cement ratio of 0.39 at 16 parts of water to 100 parts of powder. At that ratio Normet reports 30 MPa at 24 hours, 55 MPa at 3 days and 70 MPa at 28 days, with a flow-trough result of 450 mm in 6 seconds.
Shrinkage compensation provides an expansion of 0.3–1.0% (ASTM C827), which keeps the grout pressed against the underside of the bearing or plate as it hardens. Using non-reactive aggregate and low-alkali cement also reduces the risk of alkali-aggregate reaction in a grout that will sit under critical loads for decades.
Where it is used
- Production of bridge bearing plinths
- Crane rail bedding and alignment
- Grouting holding-down bolts and starter bars
- Bedding of precast concrete beams and elements
- Grouting under machinery, turbines and generator sets
- Repairs to spalled and cracked concrete
- Pumped grouting of long or hard-to-reach gaps
- Gaps from 5 mm to 75 mm thick
Key advantages
- Controlled expansion of 0.3–1.0% — non-shrink in service
- High early strength: 30 MPa at 24 hours and 55 MPa at 3 days (TDS values)
- 70 MPa compressive strength at 28 days
- Resistant to vibration and impact for dynamic equipment bases
- Can be poured, pumped, vibrated or rodded into place
- Strong bond to both steel and concrete
- Resistant to oil and water
- Chloride-free, with only clean water needed on site
Limitations & considerations
- Gap thickness should be between 5 mm and 75 mm as per the TDS
- Flow drops with time and temperature — mix enough for one continuous pour
- Do not grout below 5°C unless the area is protected; below 10°C, condition powder and water as the TDS sets out
- Mixing part bags is not recommended
- Do not add extra water when pumping; it can cause segregation and block the line
- Shelf life is six months unopened, stored at 10°C to 38°C, dry and out of sunlight
Selection & best practice
Prepare the surface first: remove loose material, degrease any oil, then wet the concrete for 2 hours and remove surplus water so it is saturated surface-dry at the time of pouring. Use a free-fall barrel mixer or pan-type paddle mixer that can take full bags. Put two thirds of the measured water in the drum, add the powder with the mixer running and mix for 1 minute, then add the rest of the water and mix for up to 4 minutes. Let the grout stand for 2–3 minutes to release air.
Normet’s strength data is based on 16 parts of water to 100 parts of powder by weight, while the mixing guidance gives 18.0–19.2 parts for a flowing mix and 15.2–17.2 parts for a trowellable mix. Settle the exact water content in a site trial against the flow and strength you need. Pour from one side only so that air is pushed out ahead of the grout, and keep the pour going until the gap is full. Cure immediately with TamCrete CCA or with polythene taped down to stop drafts.
Specifications
| Product type | High-flow, high-strength, non-shrink cementitious grout |
| Compressive strength | 30 MPa @ 24 hours; 55 MPa @ 3 days; 70 MPa @ 28 days (at 16 parts water : 100 parts powder) |
| Initial set | 2–3 hours |
| Typical density | 2,150–2,300 kg/m³ |
| Free water/cement ratio | 0.39 (16 parts water : 100 parts powder by weight) |
| Expansion | 0.3–1.0% (ASTM C827) |
| Flow trough | 450 mm in 6 seconds (DTp spec cl 2601, 6th edition) |
| Flow cone | 30–40 seconds (DTp spec cl 2601, 7th edition) |
| Chloride content | < 0.1% |
| Maximum aggregate size / gap | 2 mm aggregate; grout thickness 5–75 mm |
| Mixing water (by weight) | 18.0–19.2 parts per 100 (flowing); 15.2–17.2 parts per 100 (trowellable) |
| Packaging | 20 kg and 25 kg bags |
| Storage / shelf life | 10°C to 38°C, dry, out of direct sunlight; six months unopened |
Values as per Normet’s published TDS (Asia edition, V1ASIA18, 2018), based on laboratory tests. Download the TDS for the full data sheet.
Industry use cases
Bridges & Flyovers
Bearing plinths and bearing bedding where high early strength allows the next stage of work to move quickly.
Metro & Rail
Rail and equipment bedding where the grout must resist vibration and repeated impact.
Power Plants & Heavy Industry
Turbine, generator and compressor bases needing precise, fully supported bedding.
Precast Construction
Bedding of precast beams and grouting of starter bars at connections.
Ports & Material Handling
Crane rail bedding and alignment under heavy, moving wheel loads.
Frequently asked questions
What is the difference between TamCrete HF and TamCrete GP?
What gap thickness can TamCrete HF fill?
How strong is TamCrete HF?
Can TamCrete HF be pumped?
How should TamCrete HF be cured?
Where can I buy Normet TamCrete HF in India?
How we position Normet TamCrete HF
We put TamCrete HF forward where the grout is doing structural work under dynamic or concentrated loads — bridge bearings, turbines, crane rails — or where it has to flow a long way through a tight gap. For simpler base plate and anchor bolt work, Normet TamCrete GP is usually enough and easier to handle.
Where water is entering a pocket or hole before grouting, seal it first with Normet TamCrete Plug. For cleaning hardened grout off mixers and pumps afterwards, Normet TamCrete CR removes it without mechanical chipping. See the full Normet range for every product we supply.
More Normet grouting products
Source Normet TamCrete HF for your project
Pan India project supply from Space Arc, with technical support for trials, dosage and site work.