Master Builders Solutions MasterKure 220 WB
Acrylic-emulsion curing compound that locks moisture into fresh concrete — spray-applied, solvent-free, and compatible with the plaster, paint or tile that follows.
What is it?
A water-based, solvent-free acrylic-emulsion curing compound sprayed or rolled onto freshly finished or just-de-shuttered concrete, forming a temporary film that holds mix water in.
Where is it used?
Slabs, columns, beams, walls, pavements, airport and road concrete — anywhere continuous water curing isn’t practical, especially through Delhi NCR’s hot, windy summer pours.
Why use it?
Keeps water inside the concrete long enough for cement to hydrate fully, cutting plastic-shrinkage cracking and giving a harder, denser surface than concrete left to dry in open air.
How is it applied?
Applied as a thin, uniform coat by low-pressure spray (preferred) or roller at 0.15–0.20 kg/m², stepped up to 0.30 kg/m² in windy or low-humidity conditions, as soon as surface bleed water has gone.
About Master Builders Solutions MasterKure 220 WB
{“name”: “MasterKure 220 WB”, “slug”: “masterkure-220-wb”, “brand”: “Master Builders Solutions”, “realProduct”: “yes”, “officialSource”: “https://assets.ctfassets.net/ctspkgm1yw3s/5UpLNA09a5zrOWTSAMsVVl/c2862e637d965e99acd5df99da699b72/TDS_MasterKure220WB_EN_.pdf”, “category”: “protective-coatings-corrosion”, “metaTitle”: “MasterKure 220 WB | Acrylic Curing Compound | Space Arc”, “metaDescription”: “MasterKure 220 WB is Master Builders Solutions’ acrylic-emulsion curing compound for Indian concrete works, retaining moisture and cutting shrinkage cracks.”, “heroSubtitle”: “Acrylic-emulsion curing compound that locks moisture into fresh concrete — spray-applied, solvent-free, and compatible with the plaster, paint or tile that follows.”, “glance”: {“whatIsIt”: “A water-based, solvent-free acrylic-emulsion curing compound sprayed or rolled onto freshly finished or just-de-shuttered concrete, forming a temporary film that holds mix water in.”, “whereUsed”: “Slabs, columns, beams, walls, pavements, airport and road concrete — anywhere continuous water curing isn’t practical, especially through Delhi NCR’s hot, windy summer pours.”, “whyUse”: “Keeps water inside the concrete long enough for cement to hydrate fully, cutting plastic-shrinkage cracking and giving a harder, denser surface than concrete left to dry in open air.”, “howApplied”: “Applied as a thin, uniform coat by low-pressure spray (preferred) or roller at 0.15–0.20 kg/m², stepped up to 0.30 kg/m² in windy or low-humidity conditions, as soon as surface bleed water has gone.”}, “technicalInsight”: “The number worth watching on the data sheet is drying time — 2 hours 15 minutes to ASTM C309, the US specification for liquid membrane-forming curing compounds that Indian technical teams still benchmark against in the absence of a direct IS equivalent. That’s fast enough for a slab sprayed in the morning to usually take foot traffic from following trades the same day, which is what makes MasterKure 220 WB workable on programme-driven sites rather than just showcase pours. Specific gravity of 0.97–1.03 kg/lt and viscosity of 150–400 cP at 20°C sit in the range typical of a low-solids acrylic emulsion — thin enough to atomise cleanly through a standard airless or compression sprayer, the application method Master Builders Solutions itself recommends over rolling for a uniform, pinhole-free film. The stated 0.15–0.20 kg/m² dosage, rising to 0.30 kg/m² in open, windy conditions, is a starting coverage rate, not a fixed number — actual consumption is worth checking against a trial patch before committing a full pour’s worth of material.”, “applications”: [“Curing of freshly poured vertical and horizontal RCC elements — columns, beams, slabs and walls”, “High-rise construction where continuous water curing of upper floors isn’t practical”, “Airport, runway and other large-area field concrete”, “Road, channel and chute concrete exposed to wind and traffic”, “Hot, low-humidity, high-airflow site conditions typical of Delhi NCR’s pre-monsoon and summer pours”, “Concrete surfaces to be later plastered, painted, tiled, grouted or epoxy-coated”, “De-moulded precast elements needing immediate post-strip curing”, “Enclosed or indoor pours where hessian or ponding curing is impractical”], “advantages”: [“Solvent-free, water-based acrylic emulsion — safer to handle and store, including in enclosed pours”, “Single spray or roller pass replaces days of hessian, gunny-bag or ponding curing labour”, “ASTM C309-tested drying of around 2 hours 15 minutes lets follow-on trades move in faster”, “Dosage can be stepped up from 0.15 to 0.30 kg/m² to suit hot, windy Indian site conditions”, “Acrylic film stays compatible with subsequent plaster, paint, tile adhesive and epoxy — no need to strip it first”, “Reduces plastic-shrinkage cracking and improves surface hardness versus air-dried concrete”, “6-month shelf life and standard 20 kg / 200 kg packs fit normal site logistics”], “limitations”: [“A curing film manages moisture loss — it does not compensate for poor compaction, incorrect mix design or inadequate cover”, “Coverage must be increased in windy, low-humidity conditions; under-dosing reduces curing effectiveness”, “Uneven application can leave temporary colour blotching, which the manufacturer notes fades over subsequent days rather than disappearing instantly”, “For sensitive coating or flooring systems, a small compatibility trial before full-scale overcoating is still good practice despite the film’s stated coating-compatibility”, “Must be stored between 5°C and 30°C in sealed containers — site storage in direct sun or extreme heat shortens usable life”, “Pack sizes (20 kg can, 200 kg barrel) are geared to bulk site use, not small patch-repair quantities”], “bestPractice”: “Apply MasterKure 220 WB as soon as surface bleed water has left the concrete and it’s no longer visibly wet — spraying too early dilutes and weakens the film, spraying too late lets shrinkage cracking start before the membrane is even in place. Use a fan-nozzle sprayer for an even, continuous coat wherever the area allows; rolling is fine on vertical formed faces after de-shuttering but tends to leave a thicker, less uniform film and risks pooling in low spots. In Delhi’s hot, dry, windy months, push dosage toward the upper 0.30 kg/m² band and consider a second light pass on exposed terraces and rooftop slabs. Store drums between 5°C and 30°C out of direct sun, and run a small compatibility trial before overcoating with a specific plaster, tile adhesive or epoxy system on a critical project.”, “specs”: [{“property”: “Chemistry / Structure”, “value”: “Acrylic emulsion based, water-based, solvent-free”}, {“property”: “Appearance”, “value”: “White liquid”}, {“property”: “Specific Gravity (20°C)”, “value”: “0.97 – 1.03 kg/lt”}, {“property”: “Viscosity (20°C)”, “value”: “150 – 400 cP”}, {“property”: “Drying Time (ASTM C309)”, “value”: “2 hours 15 minutes”}, {“property”: “Coverage / Dosage”, “value”: “0.15 – 0.20 kg/m² (up to 0.30 kg/m² in windy / high-evaporation conditions)”}, {“property”: “Pack Sizes”, “value”: “20 kg can; 200 kg barrel”}, {“property”: “Shelf Life”, “value”: “6 months in unopened container, correctly stored”}, {“property”: “Storage”, “value”: “5°C to 30°C, sealed containers, out of direct sunlight”}], “useCases”: [{“sector”: “High-rise residential/commercial towers, Delhi NCR”, “detail”: “Spray-cured column and slab pours through summer construction cycles where daily water-curing of upper floors isn’t practical.”}, {“sector”: “Airport & pavement concrete”, “detail”: “Runway, apron and taxiway slabs where large exposed areas need fast, uniform curing without ponding water on trafficked surfaces.”}, {“sector”: “Industrial floor slabs pre-coating”, “detail”: “Warehouse and factory floor pours due for a later epoxy or PU floor coating, where an acrylic rather than wax cure film keeps coating adhesion straightforward.”}, {“sector”: “Precast & demoulded elements”, “detail”: “Boundary walls, precast panels and lintels sprayed immediately after de-moulding to arrest rapid moisture loss from thin sections.”}, {“sector”: “Road, channel & chute concrete”, “detail”: “Linear infrastructure pours exposed to wind and traffic where hessian or ponding curing crews can’t be sustained along the full length.”}], “faq”: [{“q”: “Is MasterKure 220 WB wax-based or acrylic-based?”, “a”: “It’s an acrylic-emulsion (resin) curing compound, not a wax emulsion — that’s the main technical difference from wax-based curing compounds like Fosroc’s Concure WB, and it’s why the manufacturer states plaster, paint, tiling and epoxy work can go directly over the cured film.”}, {“q”: “Do we need to remove the cured film before plastering or painting?”, “a”: “No — per the technical data sheet, cement- and resin-based applications (plaster, paint, tiling, epoxy) can be applied on the cured surface. We’d still recommend a small trial patch on critical projects before committing to full-scale overcoating.”}, {“q”: “How much MasterKure 220 WB do we need per square metre for a typical Delhi summer pour?”, “a”: “Standard coverage is 0.15–0.20 kg/m². In open, windy, high-evaporation conditions — common through Delhi NCR’s April–June pours — push this up to around 0.30 kg/m² for effective curing.”}, {“q”: “Spray or roller — which application method is better?”, “a”: “Spray is preferred for a uniform, pinhole-free film, especially on large slab or pavement areas. Roller application works on vertical, formed faces after de-shuttering but tends to lay down a thicker, less even coat, so watch for pooling.”}, {“q”: “Is it safe to use for basement or other enclosed pours?”, “a”: “Yes — MasterKure 220 WB is solvent-free, which is exactly why Master Builders Solutions recommends it for closed or poorly ventilated areas where a solvent-based curing compound would raise health and fire-safety concerns.”}, {“q”: “What pack sizes does Space Arc supply, and what’s the shelf life?”, “a”: “It’s supplied in 20 kg cans and 200 kg barrels, with a 6-month shelf life in an unopened container when stored between 5°C and 30°C, out of direct sunlight, as specified on the technical data sheet.”}], “positioning”: “Within Master Builders Solutions’ own range, MasterKure 220 WB is the standard water-based, solvent-free curing compound — the wider MasterKure family also runs to pigmented, high-solar-reflectance compounds better suited to large exposed slabs poured in peak summer sun, and solvent-dissolved variants for specialist substrates, so a site standardised on MasterKure can usually stay in-brand for a trickier curing condition. Against other manufacturers, Fosroc’s Concure WB is the closest equivalent Space Arc also distributes; it’s a wax-emulsion rather than an acrylic system, so a specifier already standardised on Fosroc curing compounds elsewhere on a project, or wanting the driest possible film with minimal follow-on-coating interaction, may prefer it — while MasterKure 220 WB’s acrylic chemistry is generally the safer default where plaster, paint or tile adhesive goes straight over the cured surface without an interim cleaning or abrasion step.”, “fosrocAlternative”: {“name”: “Concure WB”, “slug”: “fosroc-concure-wb”, “note”: “Specifiers already standardised on Fosroc’s wax-emulsion Concure WB elsewhere on a project may prefer it for consistency, but MasterKure 220 WB’s acrylic chemistry is generally the safer default where plaster, paint or tile adhesive goes straight over the cured surface without an interim abrasion or cleaning step.”}}
The technical insight
The number worth watching on the data sheet is drying time — 2 hours 15 minutes to ASTM C309, the US specification for liquid membrane-forming curing compounds that Indian technical teams still benchmark against in the absence of a direct IS equivalent. That’s fast enough for a slab sprayed in the morning to usually take foot traffic from following trades the same day, which is what makes MasterKure 220 WB workable on programme-driven sites rather than just showcase pours. Specific gravity of 0.97–1.03 kg/lt and viscosity of 150–400 cP at 20°C sit in the range typical of a low-solids acrylic emulsion — thin enough to atomise cleanly through a standard airless or compression sprayer, the application method Master Builders Solutions itself recommends over rolling for a uniform, pinhole-free film. The stated 0.15–0.20 kg/m² dosage, rising to 0.30 kg/m² in open, windy conditions, is a starting coverage rate, not a fixed number — actual consumption is worth checking against a trial patch before committing a full pour’s worth of material.
Where it is used
- Curing of freshly poured vertical and horizontal RCC elements — columns, beams, slabs and walls
- High-rise construction where continuous water curing of upper floors isn’t practical
- Airport, runway and other large-area field concrete
- Road, channel and chute concrete exposed to wind and traffic
- Hot, low-humidity, high-airflow site conditions typical of Delhi NCR’s pre-monsoon and summer pours
- Concrete surfaces to be later plastered, painted, tiled, grouted or epoxy-coated
- De-moulded precast elements needing immediate post-strip curing
- Enclosed or indoor pours where hessian or ponding curing is impractical
Key advantages
- Solvent-free, water-based acrylic emulsion — safer to handle and store, including in enclosed pours
- Single spray or roller pass replaces days of hessian, gunny-bag or ponding curing labour
- ASTM C309-tested drying of around 2 hours 15 minutes lets follow-on trades move in faster
- Dosage can be stepped up from 0.15 to 0.30 kg/m² to suit hot, windy Indian site conditions
- Acrylic film stays compatible with subsequent plaster, paint, tile adhesive and epoxy — no need to strip it first
- Reduces plastic-shrinkage cracking and improves surface hardness versus air-dried concrete
- 6-month shelf life and standard 20 kg / 200 kg packs fit normal site logistics
Limitations & considerations
- A curing film manages moisture loss — it does not compensate for poor compaction, incorrect mix design or inadequate cover
- Coverage must be increased in windy, low-humidity conditions; under-dosing reduces curing effectiveness
- Uneven application can leave temporary colour blotching, which the manufacturer notes fades over subsequent days rather than disappearing instantly
- For sensitive coating or flooring systems, a small compatibility trial before full-scale overcoating is still good practice despite the film’s stated coating-compatibility
- Must be stored between 5°C and 30°C in sealed containers — site storage in direct sun or extreme heat shortens usable life
- Pack sizes (20 kg can, 200 kg barrel) are geared to bulk site use, not small patch-repair quantities
Selection & best practice
Apply MasterKure 220 WB as soon as surface bleed water has left the concrete and it’s no longer visibly wet — spraying too early dilutes and weakens the film, spraying too late lets shrinkage cracking start before the membrane is even in place. Use a fan-nozzle sprayer for an even, continuous coat wherever the area allows; rolling is fine on vertical formed faces after de-shuttering but tends to leave a thicker, less uniform film and risks pooling in low spots. In Delhi’s hot, dry, windy months, push dosage toward the upper 0.30 kg/m² band and consider a second light pass on exposed terraces and rooftop slabs. Store drums between 5°C and 30°C out of direct sun, and run a small compatibility trial before overcoating with a specific plaster, tile adhesive or epoxy system on a critical project.
Specifications
| Chemistry / Structure | Acrylic emulsion based, water-based, solvent-free |
| Appearance | White liquid |
| Specific Gravity (20°C) | 0.97 – 1.03 kg/lt |
| Viscosity (20°C) | 150 – 400 cP |
| Drying Time (ASTM C309) | 2 hours 15 minutes |
| Coverage / Dosage | 0.15 – 0.20 kg/m² (up to 0.30 kg/m² in windy / high-evaporation conditions) |
| Pack Sizes | 20 kg can; 200 kg barrel |
| Shelf Life | 6 months in unopened container, correctly stored |
| Storage | 5°C to 30°C, sealed containers, out of direct sunlight |
Industry use cases
High-rise residential/commercial towers, Delhi NCR
Spray-cured column and slab pours through summer construction cycles where daily water-curing of upper floors isn’t practical.
Airport & pavement concrete
Runway, apron and taxiway slabs where large exposed areas need fast, uniform curing without ponding water on trafficked surfaces.
Industrial floor slabs pre-coating
Warehouse and factory floor pours due for a later epoxy or PU floor coating, where an acrylic rather than wax cure film keeps coating adhesion straightforward.
Precast & demoulded elements
Boundary walls, precast panels and lintels sprayed immediately after de-moulding to arrest rapid moisture loss from thin sections.
Road, channel & chute concrete
Linear infrastructure pours exposed to wind and traffic where hessian or ponding curing crews can’t be sustained along the full length.
Frequently asked questions
Is MasterKure 220 WB wax-based or acrylic-based?
Do we need to remove the cured film before plastering or painting?
How much MasterKure 220 WB do we need per square metre for a typical Delhi summer pour?
Spray or roller — which application method is better?
Is it safe to use for basement or other enclosed pours?
What pack sizes does Space Arc supply, and what’s the shelf life?
How we position Master Builders Solutions MasterKure 220 WB
Within Master Builders Solutions’ own range, MasterKure 220 WB is the standard water-based, solvent-free curing compound — the wider MasterKure family also runs to pigmented, high-solar-reflectance compounds better suited to large exposed slabs poured in peak summer sun, and solvent-dissolved variants for specialist substrates, so a site standardised on MasterKure can usually stay in-brand for a trickier curing condition. Against other manufacturers, Fosroc’s Concure WB is the closest equivalent Space Arc also distributes; it’s a wax-emulsion rather than an acrylic system, so a specifier already standardised on Fosroc curing compounds elsewhere on a project, or wanting the driest possible film with minimal follow-on-coating interaction, may prefer it — while MasterKure 220 WB’s acrylic chemistry is generally the safer default where plaster, paint or tile adhesive goes straight over the cured surface without an interim cleaning or abrasion step.
Fosroc Concure WB — Specifiers already standardised on Fosroc’s wax-emulsion Concure WB elsewhere on a project may prefer it for consistency, but MasterKure 220 WB’s acrylic chemistry is generally the safer default where plaster, paint or tile adhesive goes straight over the cured surface without an interim abrasion or cleaning step.
Related Protective Coatings products
Source Master Builders Solutions MasterKure 220 WB for your project